- Posts: 13
- Thank you received: 0
× If you have a question regarding coaxial, telephone, and building wire, power cable, insulation, extrusion, bunching, stranding, braiding, etc. post it here.
Aluminum wire adherence
- Ing Nicola Restaino
- Topic Author
- Offline
- Fresh Boarder
Less More
11 years 2 months ago #2640 by Ing Nicola Restaino
Aluminum wire adherence was created by Ing Nicola Restaino
I have a question regarding aluminum adherence in enameling aluminum wire.
Do you know how to increase aluminum adherence?
I know the surface must be cleaned and we need to use a good PRIMER coat.
But which kind of Primer?
Anything else?
Thanks in advance
Nicola
Do you know how to increase aluminum adherence?
I know the surface must be cleaned and we need to use a good PRIMER coat.
But which kind of Primer?
Anything else?
Thanks in advance
Nicola
Please Log in to join the conversation.
- Richard Burke
- Offline
- Senior Boarder
Less More
- Posts: 64
- Thank you received: 8
11 years 2 months ago #2672 by Richard Burke
Replied by Richard Burke on topic Re: Aluminum wire adherence
I have never heard of an aluminum primer coat. What I do know is that because aluminum is so soft, and so difficult to clean, that it is important that the first pass through the applicator be isolated from he remaining coats. This is especially true when using dies.
Please Log in to join the conversation.
- Willy M Hauer
- Offline
- Fresh Boarder
Less More
- Posts: 4
- Thank you received: 1
11 years 1 month ago #2673 by Willy M Hauer
Replied by Willy M Hauer on topic Re: Aluminum wire adherence
Ciao Nicola,
If you need really good surface cleanliness I would suggest you look into the Plasma Cleaner manufactured by Plasmait in Austria.
Contact:
Igor Rogelj
Commercial Director
Plasmait GmbH
M: +44 7810 810 656
T/F: +44 161 980 7485
email:i.rogelj@plasmait.com
Skype: igorrogelj
or
Primoz Eiselt
Plasmait GmbH (Head Office)
Philipsstrasse 27/C3
8403 Lebring
Austria
Tel.: +43-3182-52-475-0
Fax: +43-3182-52-475-4
email: This email address is being protected from spambots. You need JavaScript enabled to view it.
Con tanti saluti,
Willy
If you need really good surface cleanliness I would suggest you look into the Plasma Cleaner manufactured by Plasmait in Austria.
Contact:
Igor Rogelj
Commercial Director
Plasmait GmbH
M: +44 7810 810 656
T/F: +44 161 980 7485
email:i.rogelj@plasmait.com
Skype: igorrogelj
or
Primoz Eiselt
Plasmait GmbH (Head Office)
Philipsstrasse 27/C3
8403 Lebring
Austria
Tel.: +43-3182-52-475-0
Fax: +43-3182-52-475-4
email: This email address is being protected from spambots. You need JavaScript enabled to view it.
Con tanti saluti,
Willy
Please Log in to join the conversation.
- Richard Burke
- Offline
- Senior Boarder
Less More
- Posts: 64
- Thank you received: 8
11 years 1 month ago #2676 by Richard Burke
Replied by Richard Burke on topic Re: Aluminum wire adherence
Earlier I said that aluminum was hard to clean which is not really true. Aluminum adsorbs heat qucikly and it loses heat quickly. It also can oxidizes quicker and easier than copper plus it is not as visually evident. As a result, aluminum wire typically runs at a faster line speed than the same size copper wire. Depending upon the design or the pre-annealer/wire cleaner and the wire cooler, sometimes the wire will cool before it dries, leaving water droplets or residue on the wire. Another problem if you do not use treated water, you have to worry about the natural elements in the water remaining on the wire (such as caused bu hard water, etc.).
There are also systems that use an ultra sonic device between the payoff devices and the pre-annealer to help clean the bare wire, however they do not address the issues that occur between the pre-annealer wire cooler and the applicator.
Going back to the original question of a good primer; the important thing is to get a good first pass coating on the wire. In order to get that good first pass coat, it is essential that the enamel supply for the first pass be isolated from the supply for the remaining passes. if it isn't, you may end up with a coating that contains small aluminum dust and particles - metal flake paint looks great on cars, but when in insulating varnish, it reduces or eliminates the ability of the coating to insulate the wire electrically!
There are also systems that use an ultra sonic device between the payoff devices and the pre-annealer to help clean the bare wire, however they do not address the issues that occur between the pre-annealer wire cooler and the applicator.
Going back to the original question of a good primer; the important thing is to get a good first pass coating on the wire. In order to get that good first pass coat, it is essential that the enamel supply for the first pass be isolated from the supply for the remaining passes. if it isn't, you may end up with a coating that contains small aluminum dust and particles - metal flake paint looks great on cars, but when in insulating varnish, it reduces or eliminates the ability of the coating to insulate the wire electrically!